Degradation rates of GrInHy2.0 HTE modules

Description

Average degradation rates in mOhm*cm²/kh of the SOEC modules used in GrInHy2.0 plant, averaged over the runtime of the respective modules. There are 8 modules. Index "0" refers to the modules with initial stacks that were exchanges due to quality issues. Index "1" refers to replacement stacks with quality approved stacks. Runtime of initial stacks was 600 ... 9,000 h, while replacement stacks runtime was 5,000 ... 11,000 h.